Injection Molding Instabilities During Mold Cavity Filling: Orientation, Weld Lines and Trapped Air
How Does Mold Cavity Filling Influence Polymer and Fiber Orientation, Trapped Air, Surface Instabilities, and Weld-Line Quality?
Learn how fountain flow, shear, fiber orientation, trapped air and weld lines influence the quality and mechanical properties of injection-molded parts.
Introduction
Mold cavity filling is a dynamic process accompanied by a number of phenomena arising from the very nature of the polymer melt and the way it flows. The melt consists of a mixture of macromolecular chains of different lengths. As it passes through the runner system and mold cavity, it is subjected to shear while being intensively cooled by the mold walls.
Inside the cavity, the melt flows in a characteristic fountain-flow pattern. The macromolecular chains become oriented during flow and, in polymers containing fibrous reinforcement, the fibers are similarly oriented. At the same time, the advancing melt front displaces and compresses the air present in the cavity. When two melt streams meet again, a weld line is formed.
These phenomena do not occur independently. They interact, and their combined effects may change the appearance, internal structure and mechanical properties of the molded part.
This paper explains how these phenomena develop, what they affect and how they can be modeled and analyzed using Moldflow simulation tools.
1. Fountain Flow and Its Instabilities
As the melt enters the runner system and subsequently the mold cavity, its flow develops into a characteristic fountain-flow pattern.
The temperature of the runner and cavity walls is lower than the melt temperature. As soon as the melt contacts the wall, a layer of solidified polymer begins to form. As the melt progresses through the cavity or a cold runner, this frozen layer grows and simultaneously reduces the effective flow cross-section.
The flow velocity behind the melt front is therefore higher than directly at the front. At the melt front, the velocity vectors within the flow turn toward the mold wall. Material flowing through the center of the cross-section is thus progressively transported toward the melt front and subsequently deposited onto the cavity surface.

The thickness of the frozen layer depends primarily on three parameters:
- injection velocity,
- melt temperature,
- mold temperature.
Increasing these parameters generally reduces the thickness of the frozen layer.
Fountain flow also explains why many melt inhomogeneities become visible specifically at the surface of the molded part. Material from the melt front is transported toward the mold wall, where it is spread across the surface by shear.
This can result, for example, in streaks caused by changes in filler or pigment concentration. Water vapor transported to the surface may produce silver streaks. Dark streaks, on the other hand, may indicate degradation of the polymer or its additives.
Isolated spots or particles have a different character. Their cause is usually not the filling mechanism itself but material contamination.
Shear Rate and Shear Stress
Shear rate is an important parameter for understanding fountain-flow instabilities.
During conventional injection molding, the polymer melt flows under laminar conditions. Individual melt layers move relative to one another at different velocities. The layer in direct contact with the mold wall cools and solidifies rapidly, while adjacent layers continue to flow over it and further into the cavity.
Shear rate describes how rapidly flow velocity changes between adjacent melt layers across the cross-section of a runner or cavity. The highest shear rates occur close to the wall, while toward the center of the cross-section the velocity difference between adjacent layers decreases.
Shear rate is directly related to shear stress – the mechanical loading generated within the flowing melt. Shear viscosity describes the resistance of the polymer melt to flow and is defined by the relationship between shear stress and shear rate.

A polymer melt is not a fluid with constant viscosity. Its viscosity depends primarily on temperature and shear rate, but it is also affected by pressure.
If an unsuitable combination of processing conditions, part design and runner-system design causes the material-specific limits of shear rate or shear stress to be exceeded, the properties of the polymer melt may change, the polymer or its additives may degrade, and additional inhomogeneities may develop.
Tiger Skin Effect
One manifestation of fountain-flow instability is the tiger skin effect. Bands appear on the surface of the molded part, approximately perpendicular to the direction of melt flow, and are primarily visible as alternating glossy and matte areas.

The cause is a disruption of stable fountain flow. If flow velocity, shear rate, pressure or melt-front temperature decreases during filling, an initially stable flow may change into an unstable, creeping flow pattern.
Regions with different levels of polymer-structure orientation then alternate at the surface, producing visible changes in gloss.
The risk of tiger skin can be increased by an improperly designed gate, a long flow path, excessively low melt or mold temperature, or a significant decrease in flow velocity during filling.

Record Groove Effect
A different type of instability is the record groove effect. In this case, the defect does not consist merely of optical changes at the surface; actual grooves are formed.

If the melt or mold temperature is too low, or the flow velocity is unsuitable, the frozen layer at the melt front may become excessively thick. A local step is formed, over which the following melt flows. Due to its viscosity, however, the melt does not completely fill the space immediately behind this step.
Repeated formation of this mechanism produces characteristic surface grooves resembling those of a record.
The same problem can also arise from a sudden local reduction in flow velocity caused by a change in wall thickness.
2. Orientation of the Polymer Supermolecular Structure
Polymer macromolecules are not arranged in the melt as separate straight strands. Their long chains are mutually intertwined and form entanglements.
When the melt is at rest, these chains have various spatial arrangements within the material. Once the melt begins to flow, shear acts on the chains and the macromolecular structure starts to become oriented.
The strongest orientation develops in regions with the highest shear rate, particularly near the cavity or runner wall. As flow velocity increases, the degree of orientation also increases.

In semicrystalline polymers, a characteristic shish-kebab structure may develop in highly oriented regions. The oriented macromolecular chains form the basic longitudinal structure on which additional crystalline structures subsequently develop during crystallization. In the central region of the molded-part wall, by contrast, a considerably less oriented spherulitic structure may form.
The resulting molded part is therefore not homogeneous in terms of its internal structure.
Orientation occurs primarily during the filling phase. Its direction and intensity are therefore strongly influenced by part design, the melt-flow pattern and gate location.
The oriented structure may subsequently relax or recrystallize during the service life of the part. This can change the state of residual stress, dimensions and warpage of the molded part.
3. Flow Marks and Changes in Flow-Path Cross-Section
Changes in the cross-section of the runner or mold cavity are also important during melt flow.
If the melt passes from a larger cross-section into a smaller one, its velocity must increase in order to maintain the volumetric flow rate. At the same time, the shear rate increases.
A typical example is the transition from a runner into a significantly smaller gate. If the shear rate exceeds the limit for the particular polymer, degradation of the material or its additives may occur.
The same principle applies to a local reduction in wall thickness directly within the mold cavity. Typical examples are living hinges or local wall-thickness reductions beneath ribs used to reduce sink marks on visible surfaces.
If the polymer is subjected to excessive shear while passing through the restricted section, its properties may change. In a living hinge, for example, cracking may subsequently occur even though the mechanical stress during service itself does not exceed the allowable value. The cause may be material degradation that already occurred during cavity filling.
Local changes in velocity, shear rate and fountain-flow stability may also become visible as flow marks on the surface of the molded part. A flow mark is therefore not necessarily only a cosmetic defect; it may be a visible trace of a specific melt-flow history.
4. Orientation of Fibrous Reinforcement
The principle of structural orientation also applies to polymers modified with short rigid fibers, such as short glass fibers.
In regions of high shear rate, the fibers become oriented predominantly in the direction of melt flow. This typically occurs in the surface layers of the molded part. In the central region of the cross-section, fiber orientation is less ordered or even random.
Fiber orientation has a major influence on the properties of the composite material. Both mechanical properties and shrinkage depend on fiber direction, making the material anisotropic.
For glass-fiber-filled materials, for example, shrinkage parallel to the fiber orientation and shrinkage perpendicular to the fiber orientation are distinguished. The difference between these values can be significant and may subsequently contribute to part warpage.
Knowing only the nominal material properties is therefore insufficient. To predict the actual behavior of a part, the fiber orientation generated during filling of the specific cavity must also be known.
Injection molding simulation makes it possible to predict this orientation and subsequently use it in analyses of shrinkage, warpage or mechanical loading of the plastic part.
5. Trapped Air in the Mold Cavity
Every time the mold opens, the cavity fills with air. After the mold closes, the melt therefore does not enter an empty space; during filling, it must displace the air ahead of the melt front.
The mold design must allow this air to escape effectively.
If the air cannot escape quickly enough, the advancing melt front begins to compress it. The resulting back pressure may slow down filling and, in extreme cases, prevent the cavity from being completely filled.
At high compression rates, the air undergoes adiabatic heating. Its temperature may rise sufficiently to cause local polymer degradation and dark to black burn marks. This phenomenon is commonly referred to as the diesel effect.
Air does not become trapped only at the end of the flow path. Ribs, bosses, blind cavity regions and locations where several melt streams converge may also be critical.

Mold Venting
The risk of trapped air must be addressed during mold design.
Modern manufacturing technologies make it possible to produce increasingly complex cavity components from a single piece of material. However, this can eliminate the natural gaps between individual mold components through which air previously escaped.
Venting can be provided, for example, by grooves in the parting line, venting pins or suitably modified ejector pins.
A vent groove must have a sufficient cross-section to remove the required volume of air, but it must not be so deep that polymer melt enters the groove. The appropriate depth therefore depends, among other factors, on the viscosity of the material being processed.
Not only vent depth but also vent width and the continuation of the vent channel are important. The narrow section at the cavity boundary should be followed by a larger cross-section that allows air to escape freely while reducing the risk of vent contamination.
Simulation analysis makes it possible to predict air-trap locations and pressure and, with an appropriate model, also the effect of a specific venting solution.

6. How a Weld Line Forms – Weld Line and Melt Line
A weld line forms when two polymer melt streams rejoin.
This situation occurs, for example:
- when filling through multiple gates,
- when the melt flows around holes or cores,
- with non-uniform wall thickness,
- at local increases or reductions in cross-section,
- in certain box-shaped geometries where individual melt streams divide and subsequently rejoin.
Weld lines are therefore not an exceptional processing defect. They are a natural consequence of a specific cavity-filling pattern.

From the perspective of part development, four questions are essential: Where will the weld line form? How visible will it be? How is the region mechanically loaded? And can the location be effectively vented?
The character of the joining region changes as the melt streams converge.
When two melt fronts meet approximately head-on, the resulting region is referred to as a weld line. It is generally the most critical part of the joining region in terms of both appearance and mechanical properties.
As the two streams continue in a common direction and the angle at which they meet changes, the joining region develops into what is referred to as a melt line.
Weld line and melt line therefore do not represent two completely separate mechanisms. They describe different characteristics of melt-stream joining depending on the angle at which the melt fronts meet.
Both the position of the weld line and the nature of the melt-front convergence can be predicted using filling simulation.

7. What Determines Weld-Line Quality?
The fundamental problem associated with a weld line is a local reduction in mechanical properties. At the same time, the line may be visible at the surface and therefore represent an appearance defect.
Weld-line quality can be understood, in simplified terms, as the ability of two melt fronts to form a sufficiently compact material after they meet.
At the microscopic level, joining is based on the movement and mutual diffusion of macromolecular chains across the interface between the two melt streams. To achieve sufficient interpenetration, the macromolecules must retain adequate mobility.
The decisive parameters are therefore primarily:
- melt temperature at the location where the weld line forms,
- mold temperature,
- pressure and its action during the packing phase,
- injection velocity and the time at which the weld line forms,
- venting of the region.
In simple terms, the conditions must allow the two melt fronts to join sufficiently before the material solidifies.
If air remains trapped between the melt fronts, the situation becomes even more critical. A notch forms at the surface, simultaneously restricting material joining and acting as a stress concentrator. The weld line can therefore become a crack-initiation site.
Weld Lines in Fiber-Reinforced Polymers
In polymers reinforced with short glass fibers, another important factor must be considered – fiber orientation.
Fibers at the melt fronts become oriented according to the local flow conditions. When two melt fronts join, the fibers in the weld-line region may therefore be oriented unfavorably relative to the direction of future mechanical loading.
The weld line may consequently remain a mechanically critical location even when the melt temperature and pressure conditions were sufficient to join the polymer matrix.
One example is a mechanically loaded component made from polyphenylene sulfide with a high content of short glass fibers. The analysis showed that the reduction in melt-front temperature at the weld line was negligible and that pressure acted there for a sufficient period. Nevertheless, the component cracked during service.
The decisive factor was glass-fiber orientation. In the weld-line region, it resulted in a local reduction in stiffness of approximately 30% compared with the surrounding material.
This case demonstrates a fundamental difference between two problems. Venting can remove trapped air from a weld line, but it cannot change unfavorable fiber orientation.
If a critical weld line is located in a mechanically loaded region and its properties cannot be sufficiently improved by adjusting processing parameters, the design must be changed. One possible solution is to change the gate location and thereby move the weld line to a less highly loaded region.

Conclusion
The cavity-filling process determines much more than whether the mold cavity will be completely filled. Melt flow creates the material structure and determines a number of properties of the final molded part.
Fountain flow determines how material is deposited against the mold wall. Its instabilities may result in streaks, the tiger skin effect or the record groove effect. At the same time, shear during flow orients the macromolecular structure and, in composite materials, the fibrous reinforcement.
Fiber orientation creates anisotropy in mechanical properties and shrinkage and may contribute to subsequent warpage or local weakening of the part.
At the same time, the advancing melt displaces air from the cavity. If the mold design does not provide sufficient venting, trapped air may cause incomplete filling, burn marks or a significant deterioration in weld-line properties.
A weld line is the result of a specific cavity-filling pattern. Its position is determined primarily by part design and gate location, while its quality is influenced by processing conditions, venting and, in composite materials, fiber orientation.
When developing an injection-molded part, it is therefore not sufficient to ask whether a weld line will form. What matters is where it will form, under what conditions it will develop and how the region will be loaded during the actual function of the part.
Integrating plastic part design, mold design, injection molding process settings and simulation analysis makes it possible to identify and address these risks before the mold is manufactured or failures occur in serial production.
Related webinar
2 – Injection instability during cavity filling: orientation, cold welds, trapped air
Frequently asked questions
What is fountain flow of a polymer melt?
Fountain flow is the characteristic flow pattern that develops as polymer melt fills a mold cavity. Material from the center of the flow moves toward the melt front, turns toward the mold wall and is deposited at the cavity surface.
Why do melt inhomogeneities often become visible at the surface of a molded part?
Fountain flow transports material from the melt front toward the mold wall. Inhomogeneities such as local variations in filler or pigment concentration, water vapor or degraded material can therefore be deposited and spread across the surface.
What determines the thickness of the frozen layer during cavity filling?
The main parameters are injection velocity, melt temperature and mold temperature. Increasing these parameters generally reduces the thickness of the frozen layer.
Why is shear rate important during cavity filling?
Shear rate describes the velocity gradient between adjacent melt layers. It affects melt behavior, molecular and fiber orientation and, if material-specific limits are exceeded, can contribute to degradation of the polymer or its additives.
How does the tiger skin effect develop?
Tiger skin is associated with unstable fountain flow. A decrease in flow velocity, shear rate, pressure or melt-front temperature can produce alternating regions with different structural orientation, visible as changes in surface gloss.
What is the difference between the tiger skin effect and the record groove effect?
Tiger skin is primarily an optical surface effect caused by alternating gloss. The record groove effect produces actual grooves when an excessively thick frozen layer creates repeated steps at the advancing melt front.
When does orientation of the polymer macromolecular structure occur?
Orientation develops mainly during the filling phase as shear acts on the polymer chains. It is strongest in regions of high shear rate, especially near cavity and runner walls.
Why is short-glass-fiber orientation important?
Fiber orientation makes the composite material anisotropic. Mechanical properties and shrinkage depend on fiber direction, so orientation influences stiffness, warpage and local mechanical performance.
Why are material-datasheet values alone insufficient for glass-fiber-filled polymers?
Datasheet values do not describe the local fiber orientation created during filling of a specific part. Predicting actual part behavior therefore requires knowledge of the orientation generated by the real flow pattern.
Why is trapped air in the mold cavity a problem?
Compressed air creates back pressure that can slow or prevent complete filling. Adiabatic heating can also cause local polymer degradation and burn marks, known as the diesel effect.
Where can air become trapped in a mold cavity?
Air can be trapped at the end of the flow path, in ribs, bosses, blind cavity regions and at locations where several melt streams converge.
Why is trapped air particularly dangerous at a weld line?
Air between converging melt fronts can restrict material contact and chain interdiffusion. It may also create a surface notch that acts as a stress concentrator and potential crack-initiation site.
How does a weld line form?
A weld line forms when two previously separated polymer melt streams rejoin, for example after flowing around a hole or core, from multiple gates or after being divided by part geometry.
What is the difference between a weld line and a melt line?
A weld line describes the region where two melt fronts meet approximately head-on. As the streams continue in a common direction and the convergence angle changes, the joining region develops into a melt line.
What determines weld-line quality?
Key parameters include melt temperature at the joining location, mold temperature, pressure and its duration during packing, injection velocity, the time at which the line forms and effective venting.
Does a weld line always represent a mechanical problem?
Not necessarily. Its criticality depends on its location, the conditions under which it forms and the mechanical loading of that region during actual part operation.
Can good venting solve every weld-line problem?
No. Venting can remove trapped air and improve joining conditions, but it cannot correct unfavorable fiber orientation in a short-fiber-reinforced polymer.
What can be done if a weld line forms in a mechanically critical area?
If process adjustments are insufficient, the design or filling pattern must be changed. One option is to change the gate location so that the weld line moves to a less highly loaded region.
What can Moldflow predict when these problems are being investigated?
Moldflow can help predict filling behavior, flow-front development, shear conditions, air traps, weld-line position and convergence, and fiber orientation. These results can support subsequent shrinkage, warpage and mechanical analyses.
What is the most important question when evaluating a weld line?
It is not enough to ask whether a weld line will form. The engineering assessment must consider where it forms, under what conditions it develops and how the location will be loaded during actual part operation.